నైరూప్య

On the microstructural and mechanical characteristics of friction stir spot welded aa1050-o aluminum alloys

R.M.Afify, T.S.Mahmoud, S.M.Abd-Rabbo, T.A.Khalifa


In the present investigation, the effect of friction stir spot welding (FSSW) parameters, typically, the tool rotation speed and dwell time on the microstructural and mechanical characteristics offriction stir spot welds aluminum alloy AA1050-O was investigated. The results revealed that the width of the completely metallurgical-bonded region (CMBR) increases with the increasing tool rotational speed and/or the dwell time up to certain levels. Increasing the tool rotational speed and/or the dwell time above these levels reduces the width of CMBR. Increasing the CMBR width increases the tensile-shear strength of the friction stir joint. The maximum tensile-shear force found in the present study was exhibited by the weld that has the CMBR width. The peak temperature measured during FSSW increases with increasing tool rotational speed and/or the dwell time. The maximum peak temperature observed was about 562 oC at 1600 rpm and 14 s.


నిరాకరణ: ఈ సారాంశం ఆర్టిఫిషియల్ ఇంటెలిజెన్స్ టూల్స్ ఉపయోగించి అనువదించబడింది మరియు ఇంకా సమీక్షించబడలేదు లేదా నిర్ధారించబడలేదు

ఇండెక్స్ చేయబడింది

  • CASS
  • గూగుల్ స్కాలర్
  • J గేట్ తెరవండి
  • చైనా నేషనల్ నాలెడ్జ్ ఇన్‌ఫ్రాస్ట్రక్చర్ (CNKI)
  • CiteFactor
  • కాస్మోస్ IF
  • ఎలక్ట్రానిక్ జర్నల్స్ లైబ్రరీ
  • రీసెర్చ్ జర్నల్ ఇండెక్సింగ్ డైరెక్టరీ (DRJI)
  • రహస్య శోధన ఇంజిన్ ల్యాబ్‌లు
  • ICMJE

మరిన్ని చూడండి

జర్నల్ హెచ్-ఇండెక్స్

Flyer