నైరూప్య

D. C. Electrical Conductivity and Activation Energy of P-Cresol-Melamine- Formaldehyde Terpolymers

R. N. Singru, A. B. Zade and W. B. Gurnule


Terpolymers were synthesized by the condensation of p-cresol (p-C) and melamine (M) with formaldehyde (F) in the presence of 2M HCl as catalyst with varied molar ratios of reacting monomers. The electrical properties of p-CMF-1, p-CMF-2, p-CMF-3 and p-CMF-4 terpolymers were measured over a wide range of temperature (313-423 K). From the electrical conductivity of these terpolymers, activation energies of electrical conduction have been evaluated and these values lies in the range 6.36 x 10-20 – 8.23 x 10-20 J/K. The plots of log  vs. 103/T are found to be linear over a wide range of temperature, which indicate that the Wilson’s exponential law  = oexp. (Ea/kT) is obeyed. On the basis of above studies, these terpolymers cab be ranked as semiconductors.


నిరాకరణ: ఈ సారాంశం ఆర్టిఫిషియల్ ఇంటెలిజెన్స్ టూల్స్ ఉపయోగించి అనువదించబడింది మరియు ఇంకా సమీక్షించబడలేదు లేదా నిర్ధారించబడలేదు

ఇండెక్స్ చేయబడింది

  • CASS
  • గూగుల్ స్కాలర్
  • J గేట్ తెరవండి
  • చైనా నేషనల్ నాలెడ్జ్ ఇన్‌ఫ్రాస్ట్రక్చర్ (CNKI)
  • CiteFactor
  • కాస్మోస్ IF
  • ఎలక్ట్రానిక్ జర్నల్స్ లైబ్రరీ
  • రీసెర్చ్ జర్నల్ ఇండెక్సింగ్ డైరెక్టరీ (DRJI)
  • రహస్య శోధన ఇంజిన్ ల్యాబ్‌లు
  • ICMJE

మరిన్ని చూడండి

జర్నల్ హెచ్-ఇండెక్స్

Flyer